CI meas= -0.028 (Excellent) - where the CI = (1-KPDmeas/KC) KPDmeas= 0.1941,KC= 0.1889 Ncalc = 2.08 - 2.16
Optical Data:
Biaxial (+), b=2.15
Calculated Properties of Yttrocolumbite-(Y)
Electron Density:
Bulk Density (Electron Density)=5.22 gm/cc note: Specific Gravity of Yttrocolumbite-(Y) =5.93 gm/cc.
Fermion Index:
Fermion Index = 0.0024748884 Boson Index = 0.9975251116
Photoelectric:
PEYttrocolumbite-(Y) = 655.36 barns/electron U=PEYttrocolumbite-(Y) x relectron=3,419.37 barns/cc.
Radioactivity:
GRapi = 1,204,681.73 (Gamma Ray American Petroleum Institute Units)
Concentration of Yttrocolumbite-(Y) per GRapi unit = 830.09 (PPB)
Yttrocolumbite-(Y) is Radioactive as defined in 49 CFR 173.403. Greater than 70 Bq / gram.
Estimated Maximum U.S. Postal Shipping Size
(10 mRem/hr limit, Unshielded 10 cm box)
25.25 ± 6.31 grams of pure Yttrocolumbite-(Y) .
Estimated Maximum U.S. Postal Shipping Size
(10 mRem/hr limit, Unshielded 100 cm box)
2524.9 ±631.22 grams of pure Yttrocolumbite-(Y) .
Estimated Radioactivity from Yttrocolumbite-(Y) - very strong
Specimen Size Weight/Volume (Sphere) *
Calculated Activity Bequerols (Bq)
Calculated Activity Curies (Ci)
Estimated Activity GR(api)
Estimated Exposure (mRem**)/hr If Held in Hand For One Hour
1000 gm / 6.86 cm
28,728,674
7.76E-04
1,204,681.73
396.06
100 gm / 3.18 cm
2,872,867
7.76E-05
120,468.17
39.61
10 gm / 1.48 cm
287,287
7.76E-06
12,046.82
3.96
1 gm / 6.86 mm
28,729
7.76E-07
1,204.68
0.40
0.1 gm / 3.18 mm
2,873
7.76E-08
120.47
0.04
0.01 gm / 1.48 mm
287
7.76E-09
12.05
0.00
0.001 gm / 0.69 mm
29
7.76E-10
1.20
0.00
Weight of pure Yttrocolumbite-(Y) in grams (gm) and Calculated Diameter of a Sphere with a Density of 5.93 gm/cc.*
Goverment Estimate of Average Annual Exposure (
360 mRem)
** Note: 10 microsieverts/hr = 1 mRem/hr **
Max Permissable Adult Dose 50,000 mRem/yr (hands), 15,000 mRem/yr (eyes)
Lethal Dose LD(50) Exposure 400,000 to 500,000 mRem
Yttrocolumbite-(Y) Classification
Dana Class:
08.01.03.02(08)Multiple Oxides with Nb, Ta, and Ti